Welcome to Van Dykes Taxidermy. Skip directly to: main content, navigation.
 

Oropon


Oropon Directions:


Add 1/2 lb. Oropon to every 10 gallons of lukewarm water. After de-liming de-haired hides, place hides in Oropon solution. Tumble for several hours or let stand 6 to 8 hours in stationary vessel with frequent agitation. Rinse in clear water and proceed with the tanning process.


For one step de-liming and bating:


If you wish to bate in the de-liming solution (Ammonium Sulfate) add 4 ounces of Oropon to the 10 gallons of de-liming solution and mix well. Agitate skins frequently for 2 to 3 hours. Remove and rinse skins well in clear water, then begin the tanning process, starting with the pickling bath.